Isotropic wet etch: View
Process Hierarchy
Bonding
Clean
Consulting
Deposition
Doping
Etch
Anisotropic etch
Deep RIE
Isotropic etch
Miscellaneous etch
Strip
LIGA
Lift off
Lithography
Mask making
Metrology
Miscellaneous
Packaging
Polishing
Process technologies
Thermal
Unique capabilities
If you are interested in this process, either by itself or as part of a longer processing sequence, please send us email at
engineering@mems-exchange.org
or call us at (703) 262-5368
Isotropic wet etch
Process characteristics:
Depth
Depth to etch in material.
Depth
Å
µm
nm
Depth to etch in material.
unconstrained
Etchant
Specify wet etchant (if known).
Etchant
1165 PR remover
acetic acid
acetic acid/phosphoric acid/water [1:1:30]
Ashland's 16:1:1:2 Aluminum Etch
Cyantek CR-14 (acetic acid/ceric ammonium nitrate [8%:22%])
Dynasol 165
ethylenediamene pyrocatecol
HCl [2.2%]
HCl [4%]
HCl/hydrogen peroxide/water [1:1:5]
HF
HF (buffered)
HF [49%]
HF/nitric acid
HF/water [1:10]
HF/water [1:1]
HF/water [1:50]
J.T. Baker 80-15-3-2 (CMOS Grade)
J.T. Baker Buffered Oxide Etchant 5419-03 VLSI Grade
KOH
Microchrome Tech - CEP200
NaOH/hydrogen peroxide
nitric acid/HF/water [1:2:1]
other
phosphoric acid
phosphoric acid [85%]
phosphoric acid/nitric acid/acetic acid
potasium iodide/ iodine
PRS 2000
PRS 3000
sulfuric acid/hydrogen peroxide
sulfuric acid/hydrogen peroxide [4:1]
sulfuric acid/hydrogen peroxide [98:2]
sulfuric acid/hydrogen peroxide [9:1]
Transene Aluminum Etchant -Type D
Transene Aluminum Etchant Type A (phosphoric acid/nitric acid/acetic acid)
Transene Gold TFA
Transene Nichrome TFN
Transene Nickel TFB
Specify wet etchant (if known).
Material
Material to be etched.
Material
496K PMMA
950K PMMA
Alloy 42
alumina
aluminum
aluminum oxide
aluminum/copper [99.5:0.5]
aluminum/silicon [98:2]
aluminum/silicon [99:1]
aluminum/silicon/copper [98:1:1]
Arch OiR 620-7i
Arch OiR 897-10i
Arch OiR 897-12i
Arch OiR 906-17
AZ 1518
AZ 4330
AZ 4620
AZ 5214
AZ 5214e
AZ 7900
AZ 9245
AZ 9260
AZ HiR 1075
AZ nLOF 2070
AZ P4210
AZ P4400
AZ P9260
AZO
BARC
BCB 3022-63
BCB 4024-40
BCB 4026-46
Beryllium Copper
Borofloat (Schott)
borophosphosilicate glass
brass
BSG
carbon
ceramic
chromium
chromium (transparent)
chromium/aluminum
chromium/gold
chromium/gold/chromium
copper
Corning 1737
Durimide 112A
Durimide 115A
Durimide 32A
Durimide 7520
Dynachem OFPR
Foturan (Schott)
fused silica
Futurrex NR5-8000
Futurrex NR9-8000
gallium arsenide
gallium nitride
gallium phosphide
germanium
glass (Hoya)
glass (spin-on)
glass-ceramic
gold
gold (nano-porous)
gold/titanium
HR200 photoresist
indium phosphide
indium tin oxide
kapton
Kovar
lead
lithium niobate
Magnesium fluoride
Magnesium oxide
molybdenum
Nichrome
nickel
NR1-6000PY
NTO
OCG 825 35CS
OCG 897-12i
OCG 897-21i
OCG 897-7i
palladium
permalloy
phosphosilicate glass
phosphosilicate glass (low temperature)
photoresist (G-line)
PI2610
PI2611
PI2771
plating base metal
platinum
PMMA
PMMA with MMA
polyimide CG 284
polysilicon
ProTEK B1-18
ProTEK primer
Pyrex (Corning 7740)
PZT
quartz (single crystal)
Rogers R/Flex 8080
ruthenium
sapphire
SF4 Glass
Shipley 1045
Shipley 1075
Shipley 1805
Shipley 1811
Shipley 1812
Shipley 1813
Shipley 1818
Shipley 1827
Shipley 220
Shipley 3612
Shipley SPR220-3
Shipley SPR220-7
Shipley SPR700 1.2
Shipley SPR955 CM-0.9
Shipley SPR955 CM-2.1
Shipley Ultra i-123
Shipley UV210
Shipley UV6
Sichrome
silicon
silicon carbide
silicon dioxide
silicon dioxide (low temperature)
silicon nitride
silicon oxy-nitride
silver
soda lime
stainless steel
SU-8
tantalum
tantalum nitride
tantalum oxide
titanium
titanium nitride
titanium oxide
titanium/aluminum
titanium/nickel
titanium/tungsten
tungsten
vanadium
white crown
white crown (zinc-borosilicate)
Zeonor
ZEP 520
zinc
zinc oxide
zirconium dioxide
Material to be etched.
Minimum feature size (masked)
The dimension of the smallest masked feature to be protected during the etch.
Minimum feature size (masked)
Å
µm
nm
The dimension of the smallest masked feature to be protected during the etch.
unconstrained
Minimum feature size (open)
The dimension of the smallest unmasked (open) feature to be etched.
Minimum feature size (open)
Å
µm
nm
The dimension of the smallest unmasked (open) feature to be etched.
unconstrained
Sides processed
both
Equipment