Low-stress polysilicon LPCVD I (100MPa): View
Process Hierarchy
Bonding
Clean
Consulting
Deposition
Evaporation
LPCVD
Low-stress SiN deposition
Miscellaneous deposition
Oxidation
PECVD
Spin casting
Sputtering
Doping
Etch
LIGA
Lift off
Lithography
Mask making
Metrology
Miscellaneous
Packaging
Polishing
Process technologies
Thermal
Unique capabilities
If you are interested in this process, either by itself or as part of a longer processing sequence, please send us email at
engineering@mems-exchange.org
or call us at (703) 262-5368
Low-stress polysilicon LPCVD I (100MPa)
Process characteristics:
Thickness
Amount of material added to a wafer
Thickness
*
µm
nm
Amount of material added to a wafer, must be 0 .. 1 µm
0 .. 1 µm
Batch size
24
Deposition rate
Rate at which material is added to a wafer
40 Å/min
Material
polysilicon
Pressure
Pressure of process chamber during processing
0.0146 kPa
Residual stress
50 .. 100 MPa
Sides processed
both
Temperature
588 °C
Wafer size
Wafer size
100 mm
Equipment
Thermco TMX furnace (C-stack, tube #3)
Equipment characteristics:
Wafer holder
Device that holds the wafers during processing.
quartz boat
Wafer materials
List of wafer materials this tool can accept (not list of all materials, just the wafer itself).
silicon
Wafer thickness
List or range of wafer thicknesses the tool can accept
300 .. 800 µm