Photoresist developer (AZ 5214) |
|
Process characteristics: |
Depth Depth of material removed by etch process |
|
Developer Agent that reacts with masking layer (e.g., photoresist) to etch it selectively. |
AZ 400K |
Material |
AZ 5214 |
Selectivity Primary material removal rate divided by removal rates of secondary materials (i.e., factors by which primary material is removed faster than secondary materials) |
AZ 5214: 1 |
Sides processed |
both |
Wafer size |
|
Equipment |
Hood #1 |
Equipment characteristics: |
Wafer geometry Types of wafers this equipment can accept |
no-flat, 1-flat, 2-flat, notched |
Wafer holder Device that holds the wafers during processing. |
teflon |
Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
glass (category), Pyrex (Corning 7740), quartz (single crystal), silicon, silicon on insulator |
Wafer thickness List or range of wafer thicknesses the tool can accept |
100 .. 500 µm |