Batch size |
12 |
Etchant Solutions and their concentrations. |
PRS 3000 |
Material |
photoresist (category) |
Sides processed |
both |
Temperature |
80 °C |
Wafer size |
|
Equipment |
Wetbench
|
Equipment characteristics: |
Piece dimension Range of wafer piece dimensions the equipment can accept |
0 .. 4 inch |
Piece geometry Geometry of wafer pieces the equipment can accept |
triangular shard, other, rectangular, irregular, circular |
Piece thickness Range of wafer piece thickness the equipment can accept |
100 .. 1000 µm |
Wafer geometry Types of wafers this equipment can accept |
1-flat, 2-flat, notched, no-flat |
Wafer holder Device that holds the wafers during processing. |
teflon carrier |
Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
silicon |
Wafer thickness List or range of wafer thicknesses the tool can accept |
100 .. 1000 µm |