on front Polymer clean-up |
|
Ambient Ambient to which substrate is exposed during processing |
oxygen |
Etch rate |
24.4 nm/min |
Material |
polymer (category) |
Pressure Pressure of process chamber during processing |
150 mTorr |
Process duration |
150 s |
Selectivity Primary material removal rate divided by removal rates of secondary materials (i.e., factors by which primary material is removed faster than secondary materials) |
polymer (category): 1 |
Sides processed |
either |
Temperature |
50 °C |
Wafer size |
|
Equipment |
Drytek2 |
Equipment characteristics: |
Batch sizes |
100 mm: 6, 50 mm: 6, 75 mm: 6 |
Piece geometry Geometry of wafer pieces the equipment can accept |
circular, irregular, rectangular |
Piece thickness Range of wafer piece thickness the equipment can accept |
300 .. 600 µm |
Wafer holder Device that holds the wafers during processing. |
electrode |
Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
quartz (single crystal), silicon, silicon on insulator, silicon on sapphire |
Wafer thickness List or range of wafer thicknesses the tool can accept |
300 .. 600 µm |
Comments: |
|