Nickel wet etch (Low Power Deposition): View
Process Hierarchy
Bonding
Clean
Consulting
Deposition
Doping
Etch
Anisotropic etch
Deep RIE
Isotropic etch
Miscellaneous etch
Strip
LIGA
Lift off
Lithography
Mask making
Metrology
Miscellaneous
Packaging
Polishing
Process technologies
Thermal
Unique capabilities
If you are interested in this process, either by itself or as part of a longer processing sequence, please send us email at
engineering@mems-exchange.org
or call us at (703) 262-5368
Nickel wet etch (Low Power Deposition)
Process characteristics:
Depth
Depth of material removed by etch process
Depth
*
µm
nm
Depth of material removed by etch process, must be 0.01 .. 2 µm
0.01 .. 2 µm
Batch size
3
Etch rate
0.1248 µm/min
Etchant
Solutions and their concentrations.
Transene Nickel TFB
Excluded materials
gold (category), copper
Mask materials
Materials that can be used to mask etching.
photoresist (category)
Material
nickel
Selectivity
Primary material removal rate divided by removal rates of secondary materials (i.e., factors by which primary material is removed faster than secondary materials)
nickel: 1
Sides processed
both
Temperature
25 °C
Wafer size
Wafer size
100 mm
150 mm
Equipment
Air Control Microvoid
Equipment characteristics:
Wafer holder
Device that holds the wafers during processing.
teflon carrier
Wafer materials
List of wafer materials this tool can accept (not list of all materials, just the wafer itself).
silicon, silicon dioxide, Borofloat (Schott), alumina
Wafer thickness
List or range of wafer thicknesses the tool can accept
300 .. 1000 µm