on front Alumina/ Zinc Oxide (Al2O3/ZnO) alloy Atomic Layer Deposition (ALD) |
|
Process characteristics: |
Resistivity Resistivity of the alloy |
|
Temperature |
|
Thickness |
|
Batch size |
1 |
Material |
Alumina / Zinc oxide (Al2O3/ZnO) alloy |
Pressure Pressure of process chamber during processing |
1 Torr |
Relative dielectric constant |
7.5 .. 7.8 |
Sides processed |
either |
Equipment |
Viscous flow reactor |
Equipment characteristics: |
MOS clean |
no |
Piece dimension Range of wafer piece dimensions the equipment can accept |
1 .. 150 mm |
Piece geometry Geometry of wafer pieces the equipment can accept |
triangular shard, other, rectangular, irregular, circular |
Piece thickness Range of wafer piece thickness the equipment can accept |
100 .. 1000 µm |
Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
fused silica, silicon on insulator, alumina, silicon, polycarbonate |
Attachments |
ALD_summary.pdf (205.0 KB, application/pdf)- attached by ozgur (Mehmet Ozgur) on 2005-07-18 10:11
|