Photoresist strip (O2 plasma) |
|
Etch rate |
1 .. 3 µm/min |
Gas |
O2, NF3, CF4, Nitrogen |
Materials |
photoresist on silicon nitride, photoresist on silicon dioxide, photoresist on silicon |
Thickness |
0 .. 10 µm |
Wafer size |
|
Equipment |
Ulvac Enviro |
Equipment characteristics: |
Batch sizes |
150 mm: 1 |
Wafer geometry Types of wafers this equipment can accept |
1-flat |
Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
fused silica, Corning Eagle 2000, silicon, Corning 1737, silicon on insulator |
Wafer thickness List or range of wafer thicknesses the tool can accept |
300 .. 675 µm |