on front Silicon DRIE (Bosch Process) |
|
Process characteristics: |
Depth |
|
Aspect ratio |
15 |
Etch rate |
4 µm/min |
Gas |
SF6, C4F8, Argon, O2, He |
Selectivity Primary material removal rate divided by removal rates of secondary materials (i.e., factors by which primary material is removed faster than secondary materials) |
AZ 5214: 75, silicon dioxide: 150, silicon: 1 |
Sides processed |
either |
Temperature |
25 °C |
Wafer size |
|
Equipment |
STS ASE DRIE |
Equipment characteristics: |
Batch sizes |
100 mm: 1, 150 mm: 1 |
MOS clean |
no |
Wafer geometry Types of wafers this equipment can accept |
1-flat, 2-flat, notched, no-flat |
Wafer holder Device that holds the wafers during processing. |
helium clamp |
Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
silicon |
Wafer thickness List or range of wafer thicknesses the tool can accept |
250 .. 1000 µm |