Enerjet |
|
---|---|
Model | |
Type | commercial |
Comments | |
|
|
Equipment Characteristics | |
Batch sizes | 100 mm: 8, 25 .. 49 mm: 16, 50 .. 75 mm: 8 |
Wafer diameter(s) List or range of wafer diameters the tool can accept |
50 mm, 75 mm, 100 mm |
Wafer holder Device that holds the wafers during processing. |
rotating orbital |
Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
glass (category), silicon |
Wafer thickness List or range of wafer thicknesses the tool can accept |
100 .. 1000 µm |