Applied Materials Precision 5000 (chamber C)

Model
Type
Equipment Characteristics
Wafer diameter(s)
List or range of wafer diameters the tool can accept
100 mm
Wafer holder
Device that holds the wafers during processing.
mechanical clamp
Wafer materials
List of wafer materials this tool can accept (not list of all materials, just the wafer itself).
silicon, quartz (single crystal), silicon on insulator, silicon germanium
Wafer thickness
List or range of wafer thicknesses the tool can accept
350 .. 750 µm