AMRAY 3600 Field Emission SEM |
|
---|---|
Model | |
Type | commercial |
Comments | |
|
|
Equipment Characteristics | |
Batch sizes | 100 mm: 1, 125 mm: 1, 150 mm: 1, 200 mm: 1 |
Piece dimension Range of wafer piece dimensions the equipment can accept |
0 .. 8 inch |
Piece geometry Geometry of wafer pieces the equipment can accept |
circular, irregular, other, rectangular, triangular shard |
Piece thickness Range of wafer piece thickness the equipment can accept |
0 .. 1 inch |
Wafer diameter(s) List or range of wafer diameters the tool can accept |
100 mm, 125 mm, 150 mm, 200 mm |
Wafer geometry Types of wafers this equipment can accept |
1-flat, 2-flat, no-flat, notched |
Wafer holder Device that holds the wafers during processing. |
aluminum chuck |
Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
alumina, BK7, Borofloat (Schott), ceramic, copper, Corning 1737, Foturan (Schott), fused silica, gallium arsenide, gallium phosphide, germanium, glass (Hoya), glass-ceramic, indium phosphide, lithium niobate, other, Pyrex (Corning 7740), quartz (fused silica), quartz (single crystal), sapphire, silicon, silicon carbide, silicon germanium, silicon on insulator, silicon on sapphire, titanium |
Wafer thickness List or range of wafer thicknesses the tool can accept |
0 .. 1 inch |